MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC XENOY™ CL101 PC+PBT (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applications. ISO1043: PC+PBT-I.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccASTM D792
Density 1.22 g/ccISO 1183
Water Absorption 0.50 %23°C/sat; ISO 62
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.011 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0070 - 0.011 cm/cmSABIC method
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 14 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 89ISO 2039-2
Ball Indentation Hardness 82.0 MPaISO 2039-1
Tensile Strength at Break 44.0 MPa50 mm/min; ISO 527
 49.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 52.0 MPa50 mm/min; ISO 527
 53.0 MPa50 mm/min; ASTM D638
Elongation at Break 50 %50 mm/min; ISO 527
 50 %50 mm/min; ASTM D638
Elongation at Yield 4.5 %50 mm/min; ISO 527
 4.5 %50 mm/min; ASTM D638
Tensile Modulus 2050 MPa1mm/min; ISO 527
 2050 MPa50 mm/min; ASTM D638
Flexural Yield Strength 75.0 MPa1.3 mm/min, 50 mm span; ASTM D790
 75.0 MPa2 mm/min; ISO 178
Flexural Modulus 2000 MPa1.3 mm/min, 50 mm span; ASTM D790
 2000 MPa2 mm/min; ISO 178
Izod Impact, Notched 625 J/mASTM D256
 450 J/m
@Temperature -30.0 °C
ASTM D256
 600 J/m
@Temperature 0.000 °C
ASTM D256
Izod Impact, Notched (ISO) 50.0 kJ/m²80*10*4; ISO 180/1A
 25.0 kJ/m²
@Temperature -40.0 °C
80*10*4; ISO 180/1A
 35.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 30.0 kJ/m²ISO 179/2C
 58.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 20.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
 25.0 kJ/m²
@Temperature -20.0 °C
ISO 179/2C
 25.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 30CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 3.3
@Frequency 1e+6 Hz
IEC 60250
 3.3
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 18.0 kV/mm
@Thickness 1.00 mm
shorttime; IEC 60243-1
Dissipation Factor 0.0020
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 90.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 95.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 95.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Thermal Conductivity 0.180 W/m-KISO 8302
Hot Ball Pressure Test 75.0 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 105 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 105 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 83.0 °C1.8 MPa Edgew 120*10*4 sp=100mm; ISO 75/Ae
 83.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 120 °CRate B/50; ISO 306
 120 °CRate B/50; ASTM D1525
 123 °CRate B/120; ISO 306
 155 °CRate A/50; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94 by SABIC-IP
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
Nozzle Temperature 250 - 265 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 240 - 265 °C
Zone 3 250 - 270 °C
Melt Temperature 255 - 270 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 90.0 - 100 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10836 / 244303

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.