MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond UV15DC80LV-FHC One component, UV and heat curable epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Allows for curing in “shadowed out” areas
  • Cures at temperatures as low as 80°C
  • Convenient no mix system
  • Excellent physical strength properties
Product Description: Master Bond UV15DC80LV-FHC is a special dual cure epoxy based system which offers a primary cure utilizing UV light along with a secondary heat curing mechanism. This system addresses the problem of curing areas on parts that do not allow UV light curing because of “shadowing” issues. Most noteworthy is that the heat cure portion can be initiated at only 80°C rather than at the more common 125°C. Another very useful feature of a dual cure UV is that it allows for rapid fixturing and then enables the cure to be completed by adding heat. The decrease in fixture time is highly advantageous in a production environment or when fixturing is laborious or expensive. One innovative use of a dual cure UV is to fixture two optically opaque substrates, such as metals, with the UV light exposure and then completing the cure with heat. This very low viscosity system features a cationic cure mechanism (for the UV portion) and has exceptionally low shrinkage upon curing. UV15DC80LV-FHC is not oxygen inhibited and has outstanding chemical resistance to many acids, bases, fuels and solvents. It is a superb electrical insulator and bonds well to metals, glass, ceramics and most plastics. UV15DC80LV-FHC has a service temperature range of -80°F to +350°F. Straight UV curing can be accomplished for thicknesses of 0.010” to 0.020” in seconds using UV light at 365 nm with 20-40 milliwatts/cm2 of energy. Faster cures can be achieved at higher energy outputs. Areas not cured because of shadowing can be cured at 80°C for 40-60 minutes. In addition, post curing at 125-150°C for 15-30 minutes can increase the Tg from 90°C achieved by heat curing to over 125°C. The 80°C secondary cure is truly a remarkable innovation. It has wide applicability in the optical, electronic and optoelectronic industries.

Product Advantages:

  • One component system, no mixing needed
  • Dual cure capability; UV, heat, or both
  • Rapid fixturing time
  • No oxygen inhibition
  • Bonds well to a wide variety of substrates
  • Very low viscosity, no solvents or diluents

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Water Absorption <= 1.0 %
@Temperature 23.9 °C
3 month immersion
Viscosity 150 - 500 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 70
Tensile Strength >= 5000 psi
Tensile Modulus >= 350000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 3.49
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 - 65.0 µm/m-°C
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -80.0 °F
Glass Transition Temp, Tg >= 125 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.52
 
Processing PropertiesOriginal ValueComments
Shelf Life 2.00 Monthin original unopened containers
 6.00 Month
@Temperature 4.44 - 10.0 °C
Refrigerated, in original unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM5945 / 306834

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.