MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Evonik Crosslinker 200
Categories: Other Engineering Material

Material Notes: The cross-linkers of the Cross-linker 100 and 200 series are polydimethyl siloxanes comprising SiH groups in the polymer chain. The cross-linkers of the Crosslinker 200 series additionally have terminal SiH groups. Both cross-linker types are used in polyaddition silicones. Both series are available with different viscosity levels and SiH contents. Other SiH contents and viscosity levels can be delivered upon request.

Application: When working with two-component silicone formulations, it must be ensured that Pt-catalyst (e. g. Catalyst 500 series) and SiH cross-linkers are kept strictly separated. In general, the composition must be selected so that the total formulation contains approximately a double molar excess of SiH groups as compared with vinyl groups.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/cc
Viscosity 50 cP
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.403
 
Descriptive Properties
Appearanceclear, colorless liquid
Content3.2 mmol/gSiH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIL774 / 196978

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.