MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M 12056 Black 3/16" (4.8 mm) Polyurethane Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes:
  • High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement
  • Choice of medium or high density
  • Low water absorption and good solvent resistance for tough duty gasketing
  • Choice of thickness from low profile 1/16 inch to a gap-filling 1/2 inch
  • Low VOC to help meet green goals
  • Low-outgassing for electronics applications
  • Choice of five prelaminated adhesive formulations with good peel and shear strength for most surfaces including hard-to-bond plastics; all with performance at up to 250°F
  • Available with or without adhesive
  • Clean, easy die cutting and slitting
  • Low minimum order quantities
  • Custom slit widths
  • Non Adhesive foams are UL 94HBF, File E61941 Recognized Coupon

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.320 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 0.517 MPa
Elongation at Break 100 %
Compressive Strength 8.00 - 12.0 psiDeflection
Tear Strength 1.22 kg(f)/cm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 66.0 °CLong term
 121 °CShort term

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM33884 / 168631

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.