Super Oilite® is harder and of higher strength than Oilite bronze, although it has a lower speed rating in bearing applications. Oilite self-lubricating bearing products are made by a powder metallurgy process, allowing close control on the manufacturing process. They contain large interconnected pores to channel lubricants to the areas between shaft and bearing. Super Oilite is used in farm equipment, off road equipment, winches, sheaves, conveys, pulleys, etc.Oilite® is the Registered US Trademark of Beemer Precision, Inc. |
ASTM B-439-95 GR. 4; MIL-B-5687D Type 2 GR 4 |