Low dielectric and loss, high performance prepreg. 350°F Cure Developed with consistent handling and superior performance Designed for demanding electrical, radome and antennae applications Delivers superior performance with service up to 350°F with post cure Available in woven and unidirectional product forms using all fibers including carbon, quartz and S2 glass Nano-enhancement for tailored laminate properties and multi-functional performance Information provided by Renegade Materials Corporation. Renegade Materials has been acquired by Teijin. |
Cyanate ester prepreg, low dielectric loss |