MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Epoxy Technology EPO-TEK® OM125 Optical Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Product Description: EPO-TEK® OM125 is two component, high Tg, optical epoxy designed for bonding multi-mode fiber optic connectors.

Advantages & Application Notes:

  • Color coded blue for easy operator ID on the manufacturing floor.
  • A reliability test report is available when using MM fibers and MT ferrule connectors.
  • It is compatible with Telcordia GR1221 and GR326.
  • Versatility in curing from 23°C to 80°C.
  • When used in optical beam pathway, a non-blue version is available.
  • A low viscosity allows for wicking and capillary process methods. Can also be used for potting and encapsulation.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.990 g/ccPart B
 1.16 g/ccPart A
Viscosity 2400 - 5400 cP
@Temperature 23.0 °C
50 rpm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 81
Tensile Modulus 388000 psiStorage
Shear Strength 808 psiLap
 >= 6800 psiDie
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 2.00e+13 ohm-cm
Dielectric Constant 3.9
@Frequency 1000 Hz
Dissipation Factor 0.0188
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 28.0 µm/m-°CBelow Tg
 114 µm/m-°CAbove Tg
Maximum Service Temperature, Air 175 °CContinuous
 275 °CIntermittent
Minimum Service Temperature, Air -55.0 °CContinuous
 -55.0 °CIntermittent
Glass Transition Temp, Tg >= 80.0 °CDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 367 °CDegradation Temperature
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 96 %
@Wavelength 1500 nm
Spectral
 >= 97 %
@Wavelength 800 nm
Spectral
 >= 98 %
@Wavelength 1000 nm
Spectral
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 80.0 °C
Minimum Bond Line
 2.00 hour
@Temperature 65.0 °C
Minimum Bond Line
 24.0 hour
@Temperature 23.0 °C
Minimum Bond Line
Pot Life <= 60 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
 
Descriptive Properties
ColorBluePart B
 Clear/ColorlessPart A
ConsistencyPourable liquid
Mix Ratio by Weight10:3
Number of ComponentsTwo
Weight Loss0.25%200°C
 0.56%250°C
 1.43%300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOXYT144 / 141183

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.