MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Naval Brass, Arsenical, Copper Alloy, UNS C46500, H01 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: 1/4 Hard

Excellent Suitability – Soldering, Brazing, Capacity for Being Hot Formed; Good Suitability – Oxyacetylene Welding, Spot Weld, Butt Weld; Fair Suitability – Gas Shielded Arc Welding, Seam Weld, Capacity for Being Cold Worked

Common Fabrication Processes: Blanking; Drawing; Forming and Bending; Heading and Upsetting; Hot Forging and Pressing; hot heading and upsetting; Shearing

Typical Uses: Architectural Metal; Elevators; Bolts; Nuts; Rivets; Aircraft Turn buckle Barrels; Balls; Condenser Plates; Heat Exchanger Tube; Heat Sinks; Petrochemical Tanks; Plater Bar for Jewelry; Plates, Baffles; Structural Uses; Valve Stems; Welding Rod; Marine Hardware; Propeller Shafts; Fittings

Applicable Specifications: Bar – SAE J461, SAE J463; Plate – ASTM B432; Plate & Sheet - for Pressure Vessels, Condensers & Heat Exchangers ASME SB171, for Pressure Vessels, Condensers & Heat Exchangers ASTM B171/B171M; Rod – SAE J461, SAE J463

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.304 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 30T 68
@Thickness 1.02 mm
Tensile Strength 70.0 ksi
@Thickness 1.02 mm
Tensile Strength, Yield 58.0 ksi
@Thickness 1.02 mm
0.5% Ext
Elongation at Break 17 %
@Thickness 1.02 mm
Tensile Modulus 15000 ksi
Modulus of Rigidity 5600 ksi
Poissons Ratio 0.34Calculated
Machinability 30 %
Forgeability 90 %
Shear Strength >= 43.0 ksi
@Thickness 1.02 mm
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm26% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.8 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 67.0 BTU-in/hr-ft²-°F
Melting Point 1630 - 1650 °F
Solidus 1630 °F
Liquidus 1650 °F
Annealing Point 800 - 1100 °F
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 1200 - 1500 °F
 
Component Elements PropertiesOriginal ValueComments
Arsenic, As 0.020 - 0.060 %
Copper, Cu 59 - 62 %
Iron, Fe <= 0.10 %
Lead, Pb <= 0.20 %
Tin, Sn 0.50 - 1.0 %
Zinc, Zn 36.7 - 40.5 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC46500x1 / 292039

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.