Semi-crystalline Nylon 66 (PA 66) Characteristics: Super Tough, Heat Stabilized, Good Flow and Release Applications: Bearings, Gears, Connectors, Automotive Housings, Power Tool Housings Processing: Injection Molding (Melt Temperature: 500-575°F, Mold Temperature: 160-195°F) Data supplied by Albis Plastics Corporation. Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off. |