ISO Shortname: ISO 7391-PC,MLPR,(,,)-18-9 MVR (300 °C/1.2 kg) 19 cm³/10 min; impact modified; improved ultrasonic weldability; low viscosity; UV stabilized; easy release; injection molding - melt temperature 280 - 320 °C; available in opaque colors only