MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Coastal Enterprises Plus™ PBLT-15 High Density Urethane Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Description & Application: PBLT-15 is a rigid, High Density Urethane, (HDU), Tooling/Modeling board designed for Prototype Machining, Water Jet Cutting, Pattern Making, Thermoforming, Prepreg Composite Layup Tooling, Vacuum Form Tooling, Tool Path Proofing, Lost Wax Casting Masters, Master Model Making, Artistic Carving Blocks, Indoor and Outdoor Signage. PBLT Plus is made in the USA.

Information provided by Costal Enterprises Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 15.0 lb/ft³ASTM D1623
Water Absorption 0.020 %
@Time 346000 sec
by Volume; ASTM D2842
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 22ASTM D2240
Tensile Strength 395 psiASTM D1623
Elongation at Break 6.8 %
Tensile Modulus 32060 psiASTM D1623
Flexural Strength 487 psiMethod 1A; ASTM D790
Flexural Modulus 16218 psiMethod 1A; ASTM D790
Compressive Strength 510 psiASTM D1621
Compressive Modulus 20360 psiASTM D1621
Shear Modulus 3.87 ksiASTM C273
Shear Strength 326 psiASTM C273
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 1.3ASTM D1678
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µin/in-°F
Specific Heat Capacity 0.235 BTU/lb-°FASTM E1269
Maximum Service Temperature, Air 200 °FDry
Glass Transition Temp, Tg 258 °FDMA/TMA
 
Descriptive Properties
"K" Value Insulation Factor0.453ASTM C177
Closed Cell Content97%ASTM D2856
Dimensional Stability<1.2%ASTM D2126

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Elastollan® B 90 A TPUR
BASF Elastollan® S 90 A TPUR
BASF Elastollan® C 88 A TPUR
BASF Elastollan® 590 A TPUR

PCOAS018 / 187051

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.