MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Struktol PE(H)-100 PL Dispersion and Compounding Additive  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Homopolymer, non-oxidized polyethylene wax.

STRUKTOL® PE(H)-100 is a versatile polyethylene wax (homopolymer) used in natural and synthetic elastomers. It is used to improve flow and processability.
STRUKTOL® PE(H)-100 also provides good release from equipment with improved pigment dispersion and finish to molded articles.

FDA Status: 175.105; 175.125; 175.300; 176.180; 176.200; 176.210; 177.1200; 177.1210; 177.2600; 178.3570; 178.3850

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/cc
Additive Loading 1.0 - 4.0 %Will not alter the properties of vulcanizates
 
Thermal PropertiesOriginal ValueComments
Dropping Point 90.0 - 105 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 24.0 Month
 
Descriptive Properties
AppearanceWhite waxy powder

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTRUK21 / 69249

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.