Hostalen GM 5010 T3 S yellow is a high density polyethylene (HDPE), yellow colored similar RAL 1018 with light stabilizer and high melt viscosity for identification marking stripes for gas pipes made from Hostalen GM 5010 T3 black. Applications: Gas PipeInformation provided by LyondellBasell. |