MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vikas Ecotech ADDFLEX CP45 Chlorinated Paraffins
Categories: Other Engineering Material

Material Notes: Product Description: Chlorinated Parafinns are secondary & economic range of plasticizers & flexiblizer for PVC. Chlorinated Paraffin (CPS) are straight-chain hydrocarbons that have been chlorinated. Chlorinated Parafinns are produced from chlorination of paraffin made by fractions obtained from petroleum distillation. These are classified according to their carbon chain length (ranging from C10-C20) & level of chlorination (ranging from 40-70%+)

Characteristics & Usages:

  • It is used as plasticizer to impart flexibility and flame retardant property to PVC Compounds, Cables, Footwears, Flooring, Films and Sheets etc. It is used as economic replacement along with Phthalate Plasticizers. The usages ranges from across many PVC application areas
  • Cable Insulation Compounds: Garden Hoses, Flame Retardant, PVC Flexible Gardening Pipes, Pressure Pipes, Housings etc., PVC Plastisol Coating/Artificial Leather Cloth Industries, PVC extrusion/other applications, production of Plastic/Rubber, Metal Cutting/Working Fluids
CAS No: 85535-85-9

Information provided by Vikas Ecotech LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 - 1.22 g/cc
@Temperature 30.0 °C
pH 5.5 - 6.510% aqueous extract; KOR/QCD/FP-1.11
Viscosity 50 - 500 cPASTM D445
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.0010[mg KOH/g]; KOR/QCD/FP-1.5
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.47 - 1.51
 
Component Elements PropertiesOriginal ValueComments
Chlorine, Cl 44.98 - 45.2 %ISI-1448-77
 
Descriptive Properties
AppearanceClear to Pale Yellow viscous Liquid
Color<100 HUHazen, ASTM D1045-86
Thermal Stability<0.10after 4 hrs @175°C, KOR/QCD/FP-1.8
Volatile loss<3%@180°C for 4hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVICAS005 / 285418

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.