MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unitika AX-1500 Dry
Categories: Polymer; Thermoplastic; Polyarylate

Material Notes: AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in moldability and provide molded products fewer in the number of sink marks, warps, and runoffs.

Characteristics:

  • Nonreinforced heat resistance: Deflection temperature under load without reinforcement: 1.8 MPa at 150°C
  • Chemical resistance: As high as those of polyamide resins, except alkali resistance
  • Adhesiveness: Chemical resistance and adhesiveness as high as those of crystalline resins
  • Lubrication: As high as those of polyamide resins
  • Molding accuracy: Fewer in the number of sink marks and warps, and lower (less than 1/3) in water absorption than polyamide resins

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccASTM D792
Water Absorption 0.75 %
@Thickness 3.17 mm,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.010 cm/cm
@Thickness 3.00 mm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 105ASTM D785
Tensile Strength at Break 72.0 MPaASTM D638
Elongation at Break 50 %ASTM D638
Flexural Strength 103 MPaASTM D790
Flexural Modulus 2600 MPaASTM D790
Izod Impact, Notched 78.0 J/m
@Thickness 3.17 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 77.0 µm/m-°CASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 150 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 210 - 230 °C
Middle Barrel Temperature 240 - 260 °C
Front Barrel Temperature 250 - 270 °C
Nozzle Temperature 250 - 270 °C
Mold Temperature 70.0 - 90.0 °Cactual surface temp
Drying Temperature 100 °C
Dry Time 10.0 - 24.0 hour
Back Pressure 0.490 - 1.47 MPagage pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unitika AX-1500 Conditioned
Unitika AXG-1500-300 Conditioned
Unitika AX-1500W Dry
Unitika AX-1500W Conditioned
Tra-Con Tra-Bond 2143D Medium Viscosity Polyamide Epoxy Adhesive

PUNITIK891 / 177911

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.