MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics Tecknit Consil®-A 897 Silver-Aluminum Filled Silicone Elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: CONSIL-A is a silicone or fluorosilicone elastomer filled with silver-plated aluminum particles designed to achieve maximum electrical conductivity. CONSIL-A provides high shielding effectiveness with minimal galvanic corrosion. Lighter in weight than other high performance conductive elastomers, CONSIL-A provides an excellent moisture seal for enclosure joints and seams.

Typical Applications: The MILG-83528 certified compounds meet the demanding requirements of many military and aerospace systems, high frequency microwave environments and wave guide connector gaskets. EMP and TEMPEST requirements are ideal applications for CONSIL-A.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.74 - 2.26 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 63 - 77ASTM D2240
Tensile Strength >= 180 psiASTM D412
Elongation at Break 60 - 260 %ASTM D412
Tear Strength 35.0 pliASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.012 ohm-cm
Shielding Effectiveness 55 dB
@Frequency 100000 Hz
H-Field
 90 dB
@Frequency 1e+10 Hz
Plane Wave
 100 dB
@Frequency 1e+9 Hz
Plane Wave
 110 dB
@Frequency 1e+7 Hz
E-Field
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 160 °C
Minimum Service Temperature, Air -55.0 °C
 
Descriptive Properties
BinderFluorosilicone
ColorBlue
FillerSilver Plated Aluminum Particles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Boron, B
Lucas-Milhaupt BRAZE 999 Commercial Grade Fine Silver
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer
Parker Chomerics Tecknit Consil®-C 875 Silver-Copper Filled Silicone Elastomer

PCHOME384 / 131094

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.