Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15 Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extrusion of foils, when a very high matt appearance is required, as well as in the extrusion of profiles. This grade is supplied in natural only for self-coloring. Sinkral D 232/M3 meets European Standards for plastics in contact with foods. Information provided by Polimeri Europa Versalis is the Eni subsidiary containing the plastics and rubber businesses. |