MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistance

Available in: Asia Pacific and Europe

Product Applications: TECHNYL B 218L V20 noir 44 N is used in all sectors of industry, offering an excellent combination of thermal and mechanical properties. This grade is commonly used for automotive applications which require a good surface appearance and a good UV resistance, such as: - external mirror housings and door handles. This product is available in black color.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccISO 1183/A
Water Absorption 1.2 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0075 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0060 cm/cm
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPaISO 527 Type 1A
Elongation at Break 3.0 %ISO 527 Type 1A
Tensile Modulus 7000 MPaISO 527 Type 1A
Flexural Modulus 5800 MPaISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²ISO 180/1eA
Charpy Impact Unnotched 45.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 3.00e+13 ohmIEC 60093
Dielectric Constant 3.7IEC 60250
Dielectric Strength 32.0 kV/mmIEC 60243
Dissipation Factor 0.010IEC 60250
Comparative Tracking Index 450 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 35.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 242 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 230 °CISO 75/Af
Flammability, UL94 HB
@Thickness 0.800 mm
1210
 HB
@Thickness 1.60 mm
1210
Oxygen Index 23 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Feed Temperature 250 - 270 °C
Front Barrel Temperature 270 - 280 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone260-270°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRHOD739 / 137970

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.