MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Telles Mirel™ F1005 Injection Molding Grade PHA Bioplastic  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyester, TP

Material Notes: Mirel F1005 is FDA cleared for use in non-alcoholic food contact applications, from frozen food storage and microwave reheating to boiling water up to 212°F. FDA clearance includes products such as house-wares, cosmetics and medical packaging.

Mirel is suitable for a wide range of injection molded food service and packaging applications including caps and closures, and disposable items such as forks, spoons, knives, tubs, trays, jars, and consumer product applications.

About Mirel Bioplastics

Mirel is a family of bioplastic materials that have physical properties comparable to petroleum-based resins, yet are both biobased and biodegradable in natural soil and water environments, home composting systems, and industrial composting facilities, where these facilities are available. The rate and extent of Mirel's biodegradablility will depend on the size and shape of the articles made from it. However, like nearly all bioplastics and organic matter, Mirel is not designed to biodegrade in conventional landfills.

Telles is a joint venture between Metabolix and Archer Daniels Midland Company.

Key Words: Polyhydroxyalkanoate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Linear Mold Shrinkage 0.0125 - 0.0155 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 25.0 MPaASTM D638
Elongation at Break 4.0 %ASTM D638
Tensile Modulus 3000 MPaASTM D638
Flexural Strength 40.0 MPaASTM D790 A
Flexural Modulus 2000 MPaASTM D790 A
Izod Impact, Notched 26.0 J/mASTM D256 A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 132 °CASTM D648 B
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °CASTM D648 B
Vicat Softening Point 124 °CASTM 1525 B10
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 175 - 180 °CReverse Temperature Profile
Middle Barrel Temperature 170 - 175 °C
Front Barrel Temperature 165 - 170 °C
Nozzle Temperature 165 - 170 °C
Melt Temperature 160 - 165 °C
Mold Temperature 55.0 - 65.0 °C(A/B)
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
Desiccant
Back Pressure <= 3.45 MPaLow
Screw Speed <= 200 rpmSlow
 
Descriptive Properties
2nd Stage Pressure<30%of 1st Stage Pressure (Low)
Equipment Recommendation: Non-Return ValveStandard Check Ring
Equipment recommendation: Screw Profile2.2:1 to 2.6:1Low Shear GP

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Telles Mirel™ F3002 Thermoforming Grade PHA Bioplastic
Biomer P209 PHB Biodegradable Polymer
Telles Mirel™ F1006 Injection Molding Grade PHA Bioplastic
Telles Mirel™ P1003 Injection Molding Grade PHA Bioplastic
BiologiQ EcoStarch GS270 Thermoplastic Starch

PMETAA950 / 108483

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.