Side one - cured silicone rubber, 0.014 in. (0.36 mm) minimum; Substrate - Prime Coated 162 Fiberglass, 0.018 in. (0.46 mm) nominal; Side two - cured silicone rubber, 0.013 in. (0.33 mm) minimum; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.045 in ±0.004 (1.1 mm ± 0.1). The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 2299 g/m² ± 187 (67.8 oz./yd.² ± 5.5). Shelf Life: 12 months. Information provided by the manufacturer, Arlon Silicone Technologies Division. Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation. |