MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® D252/257 Linear Low Density Polyethylene Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Low Density, Linear Polyethylene Film Resin

Customer Benefits: This unique broad molecular weight distribution resin has a wide processing window and produces film with an excellent combination of toughness and tensile. D252/257 may be used straight, in blends, or coextruded with HMW-HDPE, LLDPE, and LDPE. It is especially well suited in blends with LLDPE to increase melt strength and processing rate of LLDPE. In thick gauge heavy duty applications, the benefit of the high molecular weight tail is seen in puncture resistance. Processing is excellent on many types of equipment and under a variety of conditions, including high stalk. Meets FDA regulations for food packaging below cooking temperatures. D256 contains premium stabilizer.

Applications: Heavy wall bags

Property Comments: HDPE line, 4:1 BUR, .035" gap, 8" die, 56" FLH, 240 lbs/hr, 420°F

Data provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D1505
Melt Flow 0.30 g/10 minCondition 190/2.16; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 15.0 MPa2 in per min; ASTM D882
Film Tensile Strength at Yield, TD 13.0 MPa2 in per min; ASTM D882
Film Elongation at Break, MD 500 %2 in per min; ASTM D882
Film Elongation at Break, TD 600 %2 in per min; ASTM D882
Elmendorf Tear Strength MD 95 gASTM D1922
Elmendorf Tear Strength TD 450 gASTM D1922
Dart Drop Test 350 g26 in; ASTM D1709
Film Tensile Strength at Break, MD 45.0 MPa2 in per min; ASTM D882
Film Tensile Strength at Break, TD 43.0 MPa2 in per min; ASTM D882

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 222B Polyethylene Film Grade
Borealis Borstar® FB2230 LLDPE for Film
Bamberger Polymers Bapolene® 345F Medium Density Polyethylene, Film Extrusion Grade
Borealis FG5190 Linear Low Density Polyethylene
Borealis FG5224 Linear Low Density Polyethylene

PCHEVM33 / 20323

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.