MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Starflam® X-Protect RF0067K PA66-(X+GF)30 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Starflam X-Protect RF0067K is a 30% glass fiber reinforced, flame retardant PA66 for injection molded applications. The material is halogen free and red phosphorus free.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.48 g/ccDAM; ISO 1183
Water Absorption 0.90 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.1 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 94.0 MPa50% RH; ISO 527-2
 135 MPaDAM; ISO 527-2
Elongation at Break 2.1 %DAM; ISO 527-2
 3.0 %50% RH; ISO 527-2
Tensile Modulus 7900 MPa50% RH; ISO 527-2
 10500 MPaDAM; ISO 527-2
Flexural Strength 138 MPa50% RH; ISO 178
 191 MPaDAM; ISO 178
Flexural Modulus 7500 MPa50% RH; ISO 178
 10300 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 8.50 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 8.70 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 9.60 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 10.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 11.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 51.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 51.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 53.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 53.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 55.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 61.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 12.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 12.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 32.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 34.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
Comparative Tracking Index 575 V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI >= 120 sec
@Thickness 0.800 mm
PLC 0; UL 746
 >= 120 sec
@Thickness 1.60 mm
PLC 0; UL 746
 >= 120 sec
@Thickness 3.00 mm
PLC 0; UL 746
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.800 mm
PLC 0; UL 746
 >= 120 arcs
@Thickness 1.60 mm
PLC 0; UL 746
 >= 120 arcs
@Thickness 3.00 mm
PLC 0; UL 746
 
Thermal PropertiesOriginal ValueComments
Melting Point 258 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 243 °CUnannealed, 50% RH; ISO 75-2/B
 247 °CUnannealed, DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 191 °CUnannealed, 50% RH; ISO 75-2/A
 218 °CUnannealed, DAM; ISO 75-2/A
UL RTI, Electrical 140 °C
@Thickness 0.800 mm
UL 746
 140 °C
@Thickness 1.60 mm
UL 746
 140 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 110 °C
@Thickness 0.800 mm
UL 746
 110 °C
@Thickness 1.60 mm
UL 746
 110 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 140 °C
@Thickness 0.800 mm
UL 746
 140 °C
@Thickness 1.60 mm
UL 746
 140 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-0
@Thickness 0.800 mm
UL 94
 V-0
@Thickness 1.60 mm
UL 94
 V-0
@Thickness 3.00 mm
UL 94
Oxygen Index 44 %DAM; EN ISO 4589-2
Glow Wire Ignition Temperature 800 °C
@Thickness 0.800 mm
IEC 60695-2-13
 800 °C
@Thickness 1.60 mm
IEC 60695-2-13
 825 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
IEC 60695-2-12
 960 °C
@Thickness 1.60 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 280 °CInjection
Middle Barrel Temperature 280 - 290 °CInjection
Front Barrel Temperature 260 - 280 °CInjection
Melt Temperature 270 - 290 °CInjection
Mold Temperature 40.0 - 90.0 °CInjection
Drying Temperature 80.0 °C
Dry Time 4.00 hour
 
Descriptive Properties
AdditiveFlame Retarding Agent
 Heat Stabilizer
 Release agent
AppearanceNatural Color
FeaturesFlame Retardant
 Halogen Content, None
FormsPellets
Processing MethodInjection Molding
Railway ClassificationHL3EN 45545-2; R22
 HL3EN 45545-2; R23
Smoke Density, Ds Max147EN ISO 5659-2
Smoke Toxicity, CITNLP0.58NF X 70-100-1/2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9131 / 287582

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.