MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dover Chemical DOVERPHOS S680 Distearyl Pentaerythritol Diphosphite
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Doverphos S-680 is distearyl pentaerythritol diphosphite. It is a solid phosphite that imparts outstanding color stability to polyolefins, polystyrene, rubber, ABS, PVC, polyester, and polycarbonates. It is especially synergistic with hindered phenol antioxidants. Doverphos S-680 complies with FDA regulation §178.2010-Antioxidants and stabilizers for polymers and §175-105 for adhesives. Typical use levels range from 0.10 to 0.25%.

Information provided by DoverChem

Key Words: CAS# 3806-34-6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.926 - 0.938 g/cc
@Temperature 60.0 °C
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 1.0[mgKOH/gm]
 
Optical PropertiesOriginal ValueComments
Refractive Index <= 1.459
@Temperature 60.0 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 7.8 - 8.2 %
 
Descriptive Properties
AppearanceWhite Flake

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dover Chemical DOVERNOX 76 Octadecyl 3,5-di-t-butyl-4-hydroxyhydrocinnamate
Evonik VESTOWAX® SH 105 Powder Paraffin Wax
INEOS Styrolution Terluran® GP-35 ABS
Lithium Nitrate, LiNO3
BASF Octadecyl Vinyl Ether

WDOVER049 / 217668

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.