MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax™ CB259 Thermoplastic Polyolefin Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polyolefin

Material Notes: Description: Hifax™ CB259 medium high melt flow, 1,600 MPa flexural modulus, low CLTE, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact resistance, rigidity and dimensional stability. It was designed for exterior ornamentation applications requiring stiffness and low thermal expansion characteristics. Uses: Automotive exterior parts

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccISO 1183
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 55ISO 2039-2
Hardness, Shore D 69ISO 868
Tensile Strength at Break 2180 psiISO 527-1, -2
Tensile Strength, Yield 2610 psiISO 527-1, -2
Elongation at Break 450 %ISO 527-1, -2
Elongation at Yield 8.0 %ISO 527-1, -2
Flexural Modulus 232000 psiISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
@Temperature -40.0 °C
ISO 180
 33.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Dart Drop, Total Energy 21.0 J
@Temperature -15.0 °C
Instrumented Energy at Maximum Load, Ductile Failure; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 49.0 µm/m-°C
@Temperature -30.0 - 100 °C
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 201 °FUnannealed; ISO 75B-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 127 °FUnannealed; ISO 75A-1, -2
Shrinkage 0.50 %Tool, 100x150x3.2 mm; Basell Test Method
 0.80 %
@Temperature 121 °C,
Time 3600 sec
Afterbake, 100x150x3.2 mm; Basell Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hifax™ A Thermoplastic Polyolefin Elastomer
LyondellBasell Hifax™ CA260GC Thermoplastic Polyolefin Elastomer
LyondellBasell Hifax™ CB272 Thermoplastic Polyolefin Elastomer
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer
LyondellBasell Hifax™ CB252 Thermoplastic Polyolefin Elastomer

PMO788 / 53777

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.