(Viewing data as-entered.
Click here
to return)
SABIC LNP™ LUBRICOMP™ Compound DFL34 Polycarbonate (PC)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
LNP LUBRICOMP DFL34 compound is based on Polycarbonate (PC) resin containing 20% glass fiber, 15% PTFE. Added features of this grade include: Wear Resistant.
Features: Wear resistant
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.45
g/cc
ASTM D792
Density
1.45
g/cc
ASTM D792
1.45
g/cc
ISO 1183
Water Absorption
0.10 - 0.20 %
@Time 86400 sec
ASTM D570
0.10 - 0.20 %
@Time 86400 sec
ISO 62-1
Moisture Absorption
0.0200 %
Injection Molding
0.100 - 0.200 %
23°C/50% RH/24 hrs; ASTM D570
0.100 - 0.200 %
23°C / 50% RH; ISO 62
Viscosity
5.0
cP
@Load 2.16 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow
0.0020
-
0.0040
cm/cm
SABIC method
Linear Mold Shrinkage, Transverse
0.0030
-
0.0060
cm/cm
SABIC method
Melt Flow
8.8
g/10 min
@Load 2.16 kg,
Temperature 300 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
95.0
MPa
5 mm/min; ASTM D638
97.0
MPa
5 mm/min; ISO 527
Elongation at Break
2.8 %
5 mm/min; ISO 527
3.3 %
5 mm/min; ASTM D638
Tensile Modulus
6600
MPa
5 mm/min; ASTM D638
6600
MPa
1 mm/min; ISO 527
Flexural Strength
148
MPa
1.3 mm/min, 50 mm span; ASTM D790
150
MPa
2 mm/min; ISO 178
Flexural Modulus
5600
MPa
1.3 mm/min, 50 mm span; ASTM D790
6000
MPa
2 mm/min; ISO 178
Izod Impact Notched
150
J
ASTM D256
Izod Impact, Unnotched
700
J/m
ASTM D4812
Izod Impact, Notched (ISO)
15.0
kJ/m²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
49.0
kJ/m²
80*10*4; ISO 180/1U
Charpy Impact Unnotched
61.0
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched
21.0
kJ/m²
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy
22.0
J
peak; ASTM D3763
Impact Test
7.00
J
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic
0.48
ASTM D3702 Modified: Manual
Coefficient of Friction, Static
0.64
ASTM D3702 Modified: Manual
K (wear) Factor
76.0
x 10
-10
in³-min/ft-lb-hr
Washer; ASTM D3702 Modified: Manual
Electrical Properties
Original Value
Comments
Comparative Tracking Index
175
-
250
V
UL 746A
Hot Wire Ignition, HWI
>=
120
sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI
30
-
60
arcs
@Thickness >=3.00 mm
UL 746A
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
25.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
28.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
28.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow
66.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
66.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
78.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
146
°C
Flatw 80*10*4 sp=64mm; ISO 75/Bf
147
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
142
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
143
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point
148
°C
Rate B/50; ISO 306
148
°C
Rate B/50; ASTM D1525
150
°C
Rate B/120; ISO 306
UL RTI, Electrical
80.0
°C
UL 746B
UL RTI, Mechanical with Impact
80.0
°C
UL 746B
UL RTI, Mechanical without Impact
80.0
°C
UL 746B
Flammability, UL94
V-1
@Thickness >=3.00 mm
UL 94
Processing Properties
Original Value
Comments
Zone 2
310
-
320
°C
Zone 3
320
-
330
°C
Melt Temperature
305
-
325
°C
Injection Molding
Mold Temperature
80.0
-
110
°C
Drying Temperature
120
°C
Injection Molding
Dry Time
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
Screw Speed
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH80706 / 288653
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.