MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® MP-2487C Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene MP-2487C is high performance thermoplastic elastomer designed for a variety of consumer and packaging applications requiring soft, rubber-like feel. Monprene MP-2487C is a low hardness, low density, RoHS compliant grade that is suitable for injection molding.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Contact Clarity; Good Flexibility; Good Flow; Good Moldability; Good Processability; Good Processing Stability; Good Strength; Good Tear Strength; High Flow; Light Stabilized; Low Density; Low Hardness; Low Specific Gravity; UV Absorbing

Uses: Consumer Applications; Flexible Grips; Handles; Outdoor Applications; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccASTM D792
Melt Flow 32 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40
@Time 5.00 sec
Injection Molded; ASTM D2240
 42
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 857 psi20 in/min, Flow; ASTM D412
 881 psi20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain 141 psi
@Strain 100 %
20 in/min, Across Flow; ASTM D412
 206 psi
@Strain 100 %
20 in/min, Flow; ASTM D412
 322 psi
@Strain 300 %
20 in/min, Across Flow; ASTM D412
 355 psi
@Strain 300 %
20 in/min, Flow; ASTM D412
Elongation at Break 530 %20 in/min, Across Flow; ASTM D412
 620 %20 in/min, Flow; ASTM D412
Tear Strength 109 pli20 in/min, Across Flow; ASTM D624
 124 pli20 in/min, Flow; ASTM D624
Compression Set 21 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 360 - 450 °F
Middle Barrel Temperature 370 - 460 °F
Front Barrel Temperature 380 - 470 °F
Nozzle Temperature 390 - 480 °F
Melt Temperature 390 - 480 °F
Mold Temperature 95.0 - 120 °F
Injection Pressure 200 - 800 psi
Back Pressure 25.0 - 100 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0880 / 237371

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.