MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Röhm ACRYLITE® Edgelight 8N LD96 Acrylic polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: ACRYLITE® Edgelight 8N LD96 Acrylic Molding Compound is a highly transparent light guide material based on ACRYLITE® 8N. In addition to the typical properties of ACRYLITE®, such as
  • Excellent weather resistance
  • UV-stability
  • Good flow, high mechanical strength
ACRYLITE® Edgelight 8N LD96 is developed for edge lit LED applications. The light scattering properties convert the light guide to a full illuminated panel. Furthermore, the material allows for a completely transparent view through the light guide when it is not illuminated. This opens a new degree of freedom for designers. ACRYLITE® Edgelight 8N LD96 is recommended for panels with a distance of 48 cm to 96 cm between two light injecting LED strips.

Application: Injection molding or extrusion.

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccISO 1183
Bulk Density 0.660 g/ccASTM D1895
Water Absorption <= 0.30 %ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 3.3 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 95ASTM D785
Tensile Strength 80.0 MPaASTM D638
Elongation at Break 4.0 - 6.0 %ASTM D638
Elongation at Yield 4.0 - 6.0 %ASTM D638
Tensile Modulus 3.20 GPaASTM D638
Flexural Strength 128.9 MPaASTM D790
Flexural Modulus 2.90 GPaASTM D790
Izod Impact, Notched 19.0 J/m
@Thickness 6.35 mm
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 72.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
@Thickness 6.35 mm
Annealed; ASTM D648
Vicat Softening Point 108 °C
@Load 5.10 kg
50°C/h; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003
Yellow Index <= 1.0 %ASTM E313
Transmission, Visible >= 92 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 252 °C
Mold Temperature 38.0 - 80.0 °CInjection Molding
Drying Temperature 80.0 °CPredrying
Dry Time 3.00 - 4.00 hourPredrying, Desiccant-Type Drier

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PROHM9341 / 319958

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.