Properties and applications: SIPERNAT represents a specific product range of precipitated silica, aluminum and calcium silicates. As a synthetic sodium aluminum silicate of high purity, SIPERNAT 44 MS is used as an antiblocking agent in polyolefins for excellent haze- and CoF values at high masterbatch loadings.Information provided by Evonik |