MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for PVC, Rigid Grade
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.16 - 1.65 g/ccAverage value: 1.39 g/cc Grade Count:505
Filler Content 10.0 - 20.0 %Average value: 15.0 % Grade Count:4
Volatile Organic Compounds (VOC) Content 0.300 - 0.500 g/lAverage value: 0.314 g/l Grade Count:14
Particle Size 63.0 - 250 µmAverage value: 155 µm Grade Count:14
Viscosity Test 61.0 - 116 cm³/gAverage value: 93.4 cm³/g Grade Count:13
Thickness 3000 - 12000 micronsAverage value: 6940 microns Grade Count:5
Linear Mold Shrinkage 0.000500 - 0.0120 cm/cmAverage value: 0.00394 cm/cm Grade Count:76
Melt Flow 3.50 - 54.0 g/10 minAverage value: 20.8 g/10 min Grade Count:13
Spiral Flow 53.3 - 119 cmAverage value: 78.9 cm Grade Count:55
ASTM Color -15.8 - 81.0Average value: 17.5 Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100 - 111Average value: 104 Grade Count:24
Hardness, Shore A 76.0 - 95.0Average value: 86.0 Grade Count:8
Hardness, Shore D 45.0 - 88.0Average value: 80.1 Grade Count:349
Hardness, Shore C 69.0 - 90.0Average value: 80.9 Grade Count:8
Tensile Strength, Ultimate 14.3 - 55.2 MPaAverage value: 37.0 MPa Grade Count:75
Tensile Strength, Yield 3.45 - 73.1 MPaAverage value: 45.8 MPa Grade Count:447
Elongation at Break 2.00 - 330 %Average value: 110 % Grade Count:241
Elongation at Yield 3.10 - 6.00 %Average value: 5.07 % Grade Count:6
Modulus of Elasticity 1.82 - 7.03 GPaAverage value: 2.77 GPa Grade Count:298
Flexural Yield Strength 50.7 - 104 MPaAverage value: 80.8 MPa Grade Count:289
Flexural Modulus 0.220 - 6.43 GPaAverage value: 2.79 GPa Grade Count:302
Izod Impact, Notched 0.160 - 14.0 J/cmAverage value: 4.39 J/cm Grade Count:434
 5.30 - 5.30 J/cm
@Temperature -10.0 - -10.0 °C
Average value: 2.37 J/cm Grade Count:1
 0.267 - 11.7 J/cm
@Temperature -40.0 - 10.0 °C
Average value: 2.37 J/cm Grade Count:56
 0.267 - 11.7 J/cm
@Thickness 3.18 - 3.18 mm
Average value: 2.37 J/cm Grade Count:56
Izod Impact, Unnotched 0.392 - 9.70 J/cmAverage value: 3.85 J/cm Grade Count:15
Izod Impact, Notched (ISO) 1.96 - 11.8 kJ/m²Average value: 7.36 kJ/m² Grade Count:4
Charpy Impact Unnotched NBGrade Count:5
Charpy Impact, Notched 0.250 - 1.10 J/cm²Average value: 0.582 J/cm² Grade Count:4
Dart Drop, Total Energy 19.8 - 21.9 J
@Temperature -18.0 - 0.000 °C
Average value: 20.8 J Grade Count:1
 19.8 - 21.9 J
@Thickness 1.85 - 1.85 mm
Average value: 20.8 J Grade Count:1
Dart Drop Total Energy 11.1 - 280 J/cmAverage value: 95.6 J/cm Grade Count:150
 40.0 - 66.7 J/cm
@Temperature 0.000 - 0.000 °C
Average value: 46.4 J/cm Grade Count:4
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2.00e+14 - 1.00e+16 ohm-cmAverage value: 3.82e+15 ohm-cm Grade Count:5
Dielectric Constant 2.98 - 8.00Average value: 3.96 Grade Count:3
Dissipation Factor 0.0290 - 0.0400
@Temperature 30.0 - 30.0 °C
Average value: 0.0345 Grade Count:1
 0.0290 - 0.0400
@Frequency 60.0 - 1000 Hz
Average value: 0.0345 Grade Count:1
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:5
Hot Wire Ignition, HWI 60.0 - 120 secAverage value: 90.0 sec Grade Count:5
High Amp Arc Ignition, HAI 60.0 - 120 arcsAverage value: 90.0 arcs Grade Count:5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.0 - 140 µm/m-°CAverage value: 66.2 µm/m-°C Grade Count:152
Maximum Service Temperature, Air 60.0 - 190 °CAverage value: 153 °C Grade Count:41
Deflection Temperature at 0.46 MPa (66 psi) 41.1 - 88.9 °CAverage value: 72.5 °C Grade Count:81
Deflection Temperature at 1.8 MPa (264 psi) 17.8 - 86.1 °CAverage value: 68.2 °C Grade Count:294
Vicat Softening Point 51.0 - 98.9 °CAverage value: 84.5 °C Grade Count:149
Brittleness Temperature -28.0 - 15.0 °CAverage value: -12.9 °C Grade Count:8
UL RTI, Electrical 29.4 - 105 °CAverage value: 75.3 °C Grade Count:34
UL RTI, Mechanical with Impact 10.0 - 105 °CAverage value: 63.6 °C Grade Count:29
UL RTI, Mechanical without Impact 29.4 - 105 °CAverage value: 74.2 °C Grade Count:34
Flammability, UL94 HB - 5VAGrade Count:105
Oxygen Index 24.0 - 52.0 %Average value: 31.6 % Grade Count:11
 
Optical PropertiesOriginal ValueComments
Haze 4.00 - 8.00 %Average value: 5.10 % Grade Count:10
Gloss 5.00 - 60.0 %Average value: 28.1 % Grade Count:4
Transmission, Visible 7.50 - 90.0 %Average value: 78.3 % Grade Count:51
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 - 221 °CAverage value: 186 °C Grade Count:63
Nozzle Temperature 180 - 185 °CAverage value: 180 °C Grade Count:24
Melt Temperature 177 - 216 °CAverage value: 195 °C Grade Count:224
 
Component Elements PropertiesOriginal ValueComments
Sulfate, SO4 0.0300 - 0.0500 %Average value: 0.0460 % Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PVC, Extruded
Overview of materials for PVC, Molded
Overview of materials for PVC, High Impact
Overview of materials for Chlorinated PVC (CPVC)
Overview of materials for PVC, Flexible Grade

O5646 / 78524

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.