MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco ISO 100 Saw Guide Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Saw Guide Oil is manufactured using naphthenic oils and specially selected additives balanced to reduce friction between saw and guide components in thin kerf saw equipment. These additives inhibit rust formation and pitch and resin deposits.

Oiliness properties provide excellent film strength for boundary lubrication conditions. Chevron Saw Guide Oil has tackiness properties to enable the lubricants to cling to saw components. Chevron Saw Guide Oil is designed to promote longer saw blade life in thin kerf saw equipment, when operating in severe service and reduced cooling water modes.

Chevron Saw Guide Oil solvency properties remove pitch and resin deposits, which can accumulate and create excessive temperatures.

The oil’s lubricity promotes longer saw bearing life and minimizes rust and corrosion problems, while reducing friction to allow much cooler operation.

Applications

Chevron Saw Guide Oil is specifically formulated to lubricate modern thin kerf sawing systems. Its physical properties have been tailored to meet the severe requirements of this application.

Chevron Saw Guide Oil meets or exceeds the performance requirements of most saw system manufacturers, including CAE (Newnes, McGehee), Optimil, Salem, TMT, Ukiah, and USNR (Kockums CanCar, Schurman).

The additives in these products react adversely with zinc. Do not use galvanized pipe or pot metal with these products.

Key Words: CPS Number: 255047; MSDS Number: 6954
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 22.7 °
Viscosity Measurement 55Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 502 SUS
Saybolt Viscosity at 210°F 56.7 SUS
Kinematic Viscosity at 40°C (104°F) 95 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 9.0 cStASTM D445
 
Thermal PropertiesOriginal ValueComments
Pour Point -28.0 °CASTM D97
Flash Point 190 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCHEV172 / 74787

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.