Product Description: 25 Shore A TPE (Styrenic Block Copolymer based) for injection molding and extrusion applications. This grade offers soft/tactile feel and adhesion (overmolding or co-extrusion) to ABS, PC and HIPS/PS Availability: North America Features: Acid Resistant; Alcohol Resistant; Base Resistant; Detergent Resistant; Good Adhesion; Good Colorability; Good Processability; High Elasticity; Oil Resistant; Ozone Resistant; Recyclable Material; Soft; Solvent Resistant; UV Resistant Processing Method: Extrusion; Injection Molding Information provided by Entec Polymers |