MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ravago Manufacturing Americas Compounds PP-4292 PP Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Product Description: Polypropylene Impact Copolymer; UL Recognition listing UL-94 V2; Designed for Injection molded applications; Good balance of processability and physical properties

Availability: North America

Features: Flame Retardant; Good Processability; Impact Copolymer

UL File Number: E141240

Form: Pellets

Processing Method: Injection Molding

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.948 g/ccASTM D792
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3500 psiASTM D638
Elongation at Yield 10 %ASTM D638
Flexural Modulus 160000 psiTangent; ASTM D790
Izod Impact, Notched 1.90 ft-lb/inASTM D256
Gardner Impact >= 320 in-lbGeometry GB; ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 283 °FAnnealed; ASTM D648
Flammability, UL94 V-2
@Thickness 1.52 mm
Oxygen Index 28 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 380 - 450 °FHot Runner
Rear Barrel Temperature 350 - 420 °F
Middle Barrel Temperature 350 - 420 °F
Front Barrel Temperature 340 - 420 °F
Nozzle Temperature 360 - 420 °F
Mold Temperature 80.0 - 140 °F
Drying Temperature 160 - 200 °F
Dry Time 0.000 - 8.00 hour
Back Pressure 0.000 - 100 psi
Screw Speed 50 - 150 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRAVAGO41226 / 311919

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.