System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Dow CYCLOTENE™ XU35133 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
Categories:
Polymer
Material Notes:
CYCLOTENE™ XU35133 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.
Information provided by Dow
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Viscosity Measure
34
cSt
Thickness
0.800
-
1.80
microns
Mechanical Properties
Original Value
Comments
Tensile Strength, Ultimate
78.0
-
96.0
MPa
Elongation at Break
5.5 - 10.5 %
Tensile Modulus
2.70
-
3.10
GPa
Poissons Ratio
0.34
Shear Modulus
1.01
-
1.16
GPa
Calculated
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+19
ohm-cm
Dielectric Constant
2.65
@Frequency 1.00e+9 - 2.00e+10 Hz
Dielectric Strength
530
kV/mm
Dissipation Factor
0.00080
Thermal Properties
Original Value
Comments
CTE, linear
42.0
µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity
0.290
W/m-K
Glass Transition Temp, Tg
>=
350
°C
Decomposition Temperature
350
°C
1.7% weight loss per hour
Descriptive Properties
Stress on Si MPa, Min
26 - 30
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Dow CYCLOTENE™ 3022-46 Bisbenzocyclobutene (BCB) Electronic Resin
Dow CYCLOTENE™ 4024-40 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
Dow CYCLOTENE™ XU35132 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
Dow CYCLOTENE™ XU35075 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB)
Dow CYCLOTENE™ 3022-35 Bisbenzocyclobutene (BCB) Electronic Resin
PDOW1043 / 30247
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.