MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Coosa Composites Bluewater 20 12 mm Fiberglass Reinforced Polyurethane Foam Panel
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Glass Filled

Material Notes: The Bluewater composite panels are made from high-density closed-cell polyurethane foam reinforced with continuous strand fiberglass and woven roving. They’re used for lightweight building applications that previously called for the use of plywood. The Bluewater series is ideal for projects in marine or high-humidity settings. It is also suitable for applications that require a high strength per cubic foot ratio with the added benefit of being lighter than plywood.

Bluewater 20: The lightest of the three Bluewater options, the Bluewater 20 boasts a density of 20 pounds per cubic foot and is over 45% lighter than plywood. The Bluewater 20 is often used as a semi-structural component and in other non-structural applications. The benefit of the Bluewater 20 is that it is one of the most economical options without compromising on quality and strength.

Information provided by Coosa Composites

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 20.0 lb/ft³ASTM C271
Thickness 12000 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2.60 MPaFlatwise; ASTM C297
Flexural Strength 26.6 MPaASTM D790
Flexural Modulus 1301 MPaASTM D790
Compressive Strength 3.50 MPaCore; ASTM C365
Compressive Modulus 63.1 MPaCore; ASTM C365
Shear Modulus 0.0251 GPaCore; ASTM C273
Shear Strength 2.80 MPaCore; ASTM C273

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOOS903 / 322923

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.