MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Green Dot Terratek® GDH-B1FA Bioplastic
Categories: Polymer; Renewable/Recycled Polymer

Material Notes: Product Description: Terratek® GDH-B1FA is a unique elastomeric bioplastic with a diverse range of potential applications. The bioplastic is verified to meet U.S. (ASTM D6400-04) and E.U. (EN13432) standards for compostability.

Applications: This material is suitable for injection molding, profile extrusion, sheet extrusion, blow molding, and blown film.

Information provided by Green Dot Bioplastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.23 g/ccISO 1183-1
Linear Mold Shrinkage, Flow 0.0050 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0010 in/inASTM D955
Melt Flow 57 g/10 min
@Load 2.20 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 74ISO 868
Tensile Strength, Ultimate 9.40 MPaISO 37
Elongation at Break >= 600 %ISO 37
Modulus of Elasticity 638 ksiISO 37
Tear Strength 57.0 kN/mISO 34-1
Compression Set 33 %
@Temperature 23.0 °C,
Time 79200 sec
ISO 815/ASTM D395(B)
 82 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815/ASTM D395(B)
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 330 °F
Middle Barrel Temperature 280 - 330 °F
Front Barrel Temperature 280 - 330 °F
Nozzle Temperature 280 - 300 °F
Melt Temperature <= 350 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGREEND5022 / 312293

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.