MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX679 Polyphenylene Ether + PA (PPE+Nylon) (Asia)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 679 resin is a conductive, mineral reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade is optimized to allow for primer-less electrostatic painting. NORYL GTX679 resin has improved impact / elongation, and the mineral content allows for the material to be used in structural applications such as metal and thermoset resin replacement. This material is available only in black.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Conductive,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Density 1.24 g/ccISO 1183
Moisture Absorption 0.0700 %Injection Molding
 0.700 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 3.6 %ISO 62-1
Viscosity 14 cP
@Load 5.00 kg,
Temperature 220 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0070 - 0.0090 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 16 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 61.0 MPa5 mm/min; ISO 527
 62.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 61.0 MPa5 mm/min; ISO 527
 64.0 MPa5 mm/min; ASTM D638
Elongation at Break 4.0 %5 mm/min; ASTM D638
 5.0 %5 mm/min; ISO 527
Elongation at Yield 2.0 %5 mm/min; ISO 527
 3.0 %5 mm/min; ASTM D638
Tensile Modulus 4450 MPa5 mm/min; ASTM D638
 4790 MPa1 mm/min; ISO 527
Flexural Strength 108 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 109 MPayield, 2 mm/min; ISO 178
Flexural Modulus 4000 MPa1.3 mm/min, 50 mm span; ASTM D790
 4440 MPa2 mm/min; ISO 178
Izod Impact Notched 39.0 JASTM D256
 31.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 4.00 kJ/m²80*10*4; ISO 180/1A
 3.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 3.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 7.00 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 59.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 59.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 64.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 64.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 184 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 185 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 185 °CRate B/50; ASTM D1525
 185 °CRate B/50; ISO 306
 188 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 275 - 300 °C
Zone 2 265 - 300 °C
Zone 3 270 - 300 °C
Melt Temperature 275 - 300 °CInjection Molding
Mold Temperature 65.0 - 95.0 °C
Drying Temperature 95.0 - 105 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %minimum
Back Pressure 0.300 - 1.40 MPa
Shot Size 30 - 50 %
Vent Depth 0.00130 - 0.00380 cm
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82133 / 290080

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.