MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® DW-1150 PPA, 50% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: 50% glass fiber, approved for potable water contact

Amodel® DW-1150 is a 50% glass-fiber-reinforced resin designed for high strength and stiffness and improved hydrolytic stability. This material has low moisture absorption and a low coefficient of thermal expansion, which means excellent dimensional stability. Creep resistance is also exceptional.

This grade has been approved for use with potable water in the United States, France, Germany, and the United Kingdom.

- Black: DW-1150 BK938

Markets/Uses: Plumbing / Boiler & Meter Components / Boiler Components; Plumbing / Boiler & Meter Components / Drain Valves; Plumbing / Boiler & Meter Components / Pump Housings; Plumbing / Boiler & Meter Components / Water Meters; Plumbing / Fittings & Manifolds / Fittings & Manifolds; Plumbing / Mechanical Parts / Structural Parts; Plumbing / Shower Valves & Taps / Faucet Components; Plumbing / Shower Valves & Taps / Filter Housing; Plumbing / Shower Valves & Taps / Pressure Balance Valves; Plumbing / Shower Valves & Taps / Spray Wands

Applications: Appliances; Consumer Applications; Filters; Housings; Industrial Applications; Plumbing Parts; Pump Parts; Valves/Valve Parts

Features: Chemical Resistant; Chlorine Resistant; Creep Resistant; Good Dimensional Stability; High Stiffness; High Strength; High Temperature Strength; Low Moisture Absorption

Injection notes: Mold Temperature:
- Higher tool temperatures might be required for thin wall sections
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccMethod A; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 260 MPaISO 527-2
Elongation at Break 1.9 %ISO 527-2
Tensile Modulus 18000 MPaISO 527-2
Flexural Strength 400 MPaASTM D790
Flexural Modulus 18500 MPaISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²ISO 180
Charpy Impact Unnotched 80.0 kJ/m²ISO 179
Charpy Impact, Notched 12.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 300 °CUnannealed, Flatwise; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 310 - 330 °C
Middle Barrel Temperature 315 - 330 °C
Front Barrel Temperature 325 - 335 °C
Melt Temperature 320 - 345 °CInjection
Mold Temperature 150 °C
Drying Temperature 120 °C
@Time 14400 sec
Moisture Content 0.030 - 0.060 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack; Natural Color
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4111 / 279911

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.