MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chosun Refractories SAL85 Special Alumina brick
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes:

Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.95 g/cc
Porosity 18 %
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 800 kg(f)/cm²Cold Crushing Strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.80 µm/m-°C
@Temperature 1000 °C
Shrinkage 0.00 %
@Temperature 1600 °C,
Time 7200 sec
 
Component Elements PropertiesOriginal ValueComments
Al2O3 86 %
Fe2O3 0.60 %
 
Descriptive Properties
Main ApplicationLime Kiln, Cement kiln, Various Rotary kiln, Reheating furnace, Soaking Pits, Various high-temp. furnace
Refractories Under Load(2kg/cm²,T2°C)1,700
Refractoriness (SK)40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Pyro-Bloc® Zirconia Fibre Thermal Ceramic
Overview of materials for Acetal Copolymer, PTFE Filled
Morgan Advanced Ceramics Pyro-Bloc® Standard Fibre Thermal Ceramic
Copper, Cu; Cold-Worked
Concrete; Stone, 1-2-4 Mix

CCHOS011 / 123955

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.