MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics GBC-96% Alumina 96-RH/SV Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: High purity alumina ceramic with excellent mechanical, electrical, thermal, and chemical properties.

Prime Features:

  • Superior electrical properties
  • High mechanical strength and wear resistance
  • Moly-manganese metallizable
  • Chemical and corrosion resistance
  • Excellent dielectric
Typical Applications:
  • Electrical inductors
  • Lids and Covers
  • Automotive
  • Switches
  • Bushings
  • Seal rings
  • Pump seals
  • Electronic packages
  • Bearings
  • Wear resistance components
  • Severe environments
  • Military
  • General industrial duties requiring excellent mechanical, electrical, and thermal properties
Production Capabilities:
  • High volume production at low cost
  • Tight tolerance pressed alumina parts
  • Multi-cavity tooling
  • Simple to complex geometries and multilevel configurations
  • Sub-miniature designs
  • Precise material and batch control

Information provided by Morgan Advanced Materials

Key Words: 96-RH/SV
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.70 g/cc
Open Porosity 0.00 %fully dense, % nominal, apparent
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 9.0
Tensile Strength 30000 psi
Compressive Strength 300000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmat RT
Dielectric Constant 9.3
@Frequency 1e+6 Hz
at RT
Dielectric Strength 230 V/mil
Dissipation Factor 0.00040
@Frequency 1e+6 Hz
at RT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.60 µm/m-°C
@Temperature 25.0 - 300 °C
Thermal Conductivity 20.5 W/m-Kat RT
 
Component Elements PropertiesOriginal ValueComments
Al2O3 96 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec CeramCool® Rubalit® 708 Alumina, 96%
CeramTec Rubalit® 708 Alumina, 96%
Alumina, alpha Al2O3, 99.5%
Alumina, alpha Al2O3, 96%
Alcoa MIC-6 Aluminum Mold Alloy

CMORF5017 / 200255

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.