MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® IN-22946DV XRD2 Thermoplastic Vulcanizate Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene IN-22946DV XRD2 is a high performance thermoplastic elastomer vulcanizate used in industrial applications. Monprene IN-22946DV XRD2 is a low density, high hardness, RoHS compliant exhibiting excellent UV absorbing characteristics. This grade can be processed by extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Abrasion Resistant; Filled; Good Melt Strength; Good Processability; Good Processing Stability; High Hardness; Light Stabilized; Low Flow; Low Density; Low Specific Gravity; Lubricated; Slip; UV Absorbing

Uses: Capstock; Gaskets; Glazing; Grommets; Plugs; Shock Absorbing Pads; Tubing; Weather-stripping

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Viscosity 320 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 4.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 45
@Time 15.0 sec
Injection Molded; ISO 868
 47
@Time 5.00 sec
Injection Molded; ISO 868
 49
@Time 1.00 sec
Injection Molded; ISO 868
Tensile Strength at Break 1810 psi20 in/min, Across Flow; ISO 37
 2180 psi20 in/min, Flow; ISO 37
Tensile Stress at Strain 1260 psi
@Strain 100 %
20 in/min, Across Flow; ISO 37
 1820 psi
@Strain 100 %
20 in/min, Flow; ISO 37
Elongation at Break 490 %20 in/min, Flow; ISO 37
 580 %20 in/min, Across Flow; ISO 37
Tear Strength 370 pli20 in/min, Flow; ISO 34-1
 770 pli20 in/min, Across Flow; ISO 34-1
Compression Set 38 %
@Temperature 22.8 °C,
Time 79200 sec
Type A; ISO 815
 62 %
@Temperature 70.0 °C,
Time 79200 sec
Type A; ISO 815
 79 %
@Temperature 90.0 °C,
Time 252000 sec
Type A; ISO 815
 97 %
@Temperature 125 °C,
Time 252000 sec
Type A; ISO 815
 
Processing PropertiesOriginal ValueComments
Zone 1 330 - 400 °F
Zone 2 340 - 410 °F
Zone 3 350 - 420 °F
Zone 4 351 - 421 °F
Zone 5 360 - 430 °F
Die Temperature 374 - 440 °F
Screw Speed 30 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0865 / 237356

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.