Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber. Sarcon GTR is a composite of Heat Conductive Silicone Rubber and fiberglass. Information provided by Fujipoly Industries |