MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Garlock 9900 Compressed Graphite Fiber Gasketing, Nitrile Binder
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Rubber or Thermoset Elastomer (TSE)

Material Notes: Graphite fibers with a nitrile binder.
  • Graphite fiber gasketing withstands extreme temperatures and pressures, as well as many chemicals
  • Passed Garlock Fire tests, and is ABS Fire Safe Type Approved
  • Long-lasting seal - Unique manufacturing process minimizes cold flow and creep relaxation problems
  • Ideal for standard ANSI flanged connectors, as well as turbine crossover piping connectors
  • Multiple applications in power generation, chemical processing, hydrocarbon processing, and other industries
Media: Steam, oils, grease, water, heat transfer fluids

Information provided by Garlock Rubber Technologies

Key Words: butadiene acrylonitrile
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 110 lb/ft³
Permeability 0.015Gas Permeability, cc/min; DIN 3535 Part 4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1800 psiacross grain; ASTM F152
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength <= 2.00 V/mil
@Thickness 1.59 mm
Unconditioned; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1000 °F
 650 °F
@Pressure 13.8 MPa
Continuous
Minimum Service Temperature, Air -100 °F
 
Descriptive Properties
ColorMahogany
Compressibility, %7-17ASTM F36
Creep Relaxation, %9ASTM F38
Sealability ASTM F37B, ml/hr0.1ASTM Fuel A
 0.1Nitrogen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Garlock 9800 Compressed Carbon Fiber Gasketing, SBR Binder
Garlock 9850 Compressed Carbon Fiber Gasketing, Nitrile Binder
Fibre Glast 3101 3K, 2x2 Twill Weave Prepreg Carbon Fiber Fabric
DuPont Mobility and Materials Vespel® CP-9800 Carbon Fiber and Epoxy Composite, Ultra-high modulus end effectors

PGARL846 / 157506

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.