MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carmel Olefins Capilene® CL 50 E Polypropylene Film Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: CAPILENE® CL 50 E is a specialty soft polypropylene combining typical advantages of polypropylene random and heterophasic copolymers. Features: Very low flexural modulus, Excellent impact at sub-zero temperature, Very low stress whitening, High gloss, Excellent transparency, Basic additive package. Uses: Detergent and cosmetics, clear containers, High clarity films, Corrugated sheets, Profiles. Processing Methods: Injection molding, Compounding, Cast film extrusion, Thermoforming.

Information provided by Carmel Olefins Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 50.0 micronsAs Tested
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 15.0 MPa
@Thickness 0.0500 mm
cast film; ISO 527-3
Film Tensile Strength at Yield, TD 15.0 MPa
@Thickness 0.0500 mm
cast film; ISO 527-3
Film Elongation at Break, MD 470 %
@Thickness 0.0500 mm
cast film; ISO 527-3
Film Elongation at Break, TD 1190 %
@Thickness 0.0500 mm
cast film; ISO 527-3
Film Elongation at Yield, MD 13 %
@Thickness 0.0500 mm
cast film; ISO 527-3
Film Elongation at Yield, TD 15 %
@Thickness 0.0500 mm
cast film; ISO 527-3
Flexural Modulus 450 MPa5mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature -20.0 °C
ISO 180
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 180
Film Tensile Strength at Break, MD 39.0 MPa
@Thickness 0.0500 mm
cast film; ISO 527-3
Film Tensile Strength at Break, TD 41.0 MPa
@Thickness 0.0500 mm
cast film; ISO 527-3
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °CISO 75-2
Vicat Softening Point 118 °C
@Load 1.02 kg
ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 0.80 %
@Thickness 0.0500 mm
film; ASTM D1003
 35 %
@Thickness 1.00 mm
plaque; ASTM D1003
Gloss 91 %
@Thickness 0.0500 mm
45°, cast film; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCARM816 / 249036

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.