Stood® 5 is a high carbon, chromium, tungsten, iron, cobalt-base centrifugally cast alloy. This alloy is basically a modification of Stood 1 where good wear properties are required and greater resistance to impact and thermal shock is required. Recommended for steel mill guide roll applications. Information provided by Deloro Stellite Inc. Product of former Deloro Stellite Inc. |