Applications PETROTHENE NA 345-009 is a low density homopolymer resin designed for blow molding applications. Excellent clarity combined with strength and high stiffness makes NA 345-009 an ideal choice for flexible containers, squeeze bottles and toys.
Regulatory Status NA 345-009 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply.
Processing Techniques Specific recommendations for processing NA 345-009 can only be made when the processing conditions, equipment and end use are known.This product is from the former Equistar product line. |