MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Pro-fax SD242 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: short cycle times for high productivity, good cold impact resistance, good stiffness and impact balance, high flow ease of mold filling and minimum warpage, low odor and low taste transfer, FDA acceptable

Applications: food and medical containers, closures, lids, overcaps, housewares, consumer products

Meets FDA requirements in 21 CFR 177.1520 for all food contact, excluding cooking applications.

Description: Pro-fax SC242 nucleated, easy molding, high melt flow, medium impact polypropylene copolymer resin is designed for thin-wall applications requiring fat cycling and an excellent stiffness/impact balance. This resin is available in pellet form. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL. It has a UL yellow card RTI, which applies to all natural colors.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792B
Melt Flow 35 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 28.0 MPaASTM D638
Elongation at Yield 5.0 %ASTM D638
Flexural Modulus, 1% Secant 1.40 GPa0.05 in/min; ASTM D790A
Izod Impact, Notched 0.700 J/cmASTM D256A
Impact Test 20.0 J
@Temperature 5.00 °C
Montell drop weight impact strength
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CASTM D648
UL RTI, Mechanical with Impact 65.0 °C
@Thickness >=1.50 mm
Flammability, UL94 HB
@Thickness >=1.50 mm
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax SB891 Polypropylene Impact Copolymer
LyondellBasell Pro-fax 8523 Polypropylene Impact Copolymer
LyondellBasell Montell SE191 Polypropylene Impact Copolymer
LyondellBasell Pro-fax SV152 Polypropylene Impact Copolymer
LyondellBasell Pro-fax SV258 Polypropylene Impact Copolymer

PMO240 / 53569

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.