MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
TBA ECP 210 Colorable Magnetically Detectable Polypropylene for Injection Molding and Extrusion
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade; Polypropylene, Molded

Material Notes: ECP 210 is a magnetic compound based on special blends of magnetic additive compounded into PP in such a way as to optimize physical and magnetic properties. Used in the food processing industries where detection of foreign body plastics is required. Normally supplied as a blue colored or natural pelleted compound.

Applications: ECP 210 is recommended for packaging, handling, transportation applications where magnetic detection requirements exist.

Information provided by TBA Protective Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 12.7 MPa
Elongation at Break 175.4 %
Flexural Strength 25.4 MPa
Flexural Modulus 1102 MPa
Izod Impact, Notched (ISO) 23.8 kJ/m²
 
Processing PropertiesOriginal ValueComments
Processing Temperature 220 - 230 °CCylinder
Mold Temperature 25.0 - 80.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTBA013 / 281491

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.