Key Properties Excellent balance of chemical, electrical and mechanical properties. Semi-flexible,tough system. Ease of use. Applications Bonds difficult-to-bond substrates and dissimilar materials including most metals, wood, plastics, rubber, urethane and concrete. Survives harsh environments, particularly moisture, harsh chemical, marine and subsea. Exceptional performance as a universal adhesive for industrial applications. Can be applied to oily surfaces. Will cure underwater. Ambient 24 hour or accelerated thermal cure. Information provided by Reltek LLC |