Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injection molding of tough
medium-walled articles. Designation: Thermoplastics ISO 2897-PS-I,G,093-03-10-18 Applications: Typical uses are thermoformed food packaging as disposable tumblers, flatwares, yoghurt cups, lids. Injection molding of technical items, shoe heels, reels. R 850E is certified UL94 HB "all colors" at 1.5 mm (UL file E83071).
This grade in natural version complies by composition with the requirements set
by the main Regulations for plastic materials intended for food contact (included
the EEC Directive 90/128 and following amendments). Information provided by Polimeri Europa Versalis is the Eni subsidiary containing the plastics and rubber businesses. |