MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Y-TZP Y2O3 Stabilized Zirconia
Categories: Ceramic; Oxide

Material Notes: Ultra fine grain, with very high mechanical strength, plus superior corrosion and abrasion resistance.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 6.00 g/ccFired
Porosity 0.00 %Apparent, fully dense
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 45 N 80
Vickers Microhardness 12500MPa, at Hv 0.5kg
Modulus of Elasticity 200 GPa
@Temperature 20.0 °C
Flexural Strength 800 - 900 MPa
@Temperature 20.0 °C
3-point
Fracture Toughness 10.0 MPa-m½
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.00 - 10.6 µm/m-°C
@Temperature 20.0 °C
 9.00 - 10.9 µm/m-°C
@Temperature 800 °C
Specific Heat Capacity 0.610 J/g-°C
Thermal Conductivity 2.90 W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air 200 °C
 
Descriptive Properties
Thermal Downshock260Change in °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CeramTec MZ BE Zirconia 3Y-TZP, Dental Grade
China-Yixing Longly Refractories Zirconia Ceramics
AK Steel 316 Austenitic Stainless steel
CoorsTek ZDY Yttria Fully Stabilized Zirconia
MarkeTech Aluminum Oxide Ceramic - Alumina 99.5%

CMORG32 / 90410

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.